MAGNETIC POWDER AND MAGNETIC RECORDING MEDIUM USING SAME, AND SURFACE TREATMENT METHOD FOR MAGNETIC

2022-07-31 2080 227K 0
PROBLEM TO BE SOLVED : To provide a magnetic powder which is scattered well in a resin coating even if the magnetic powder comprises nanoparticulates having a diameter of less than 80 nm, in some cases, less than 50 nm when the magnetic power is turned into the form of a coating to form a magnetic layer for a magnetic recording medium, and which has an excellent storing stability while maintaining excellent magnetic characteristics. SOLUTION : The magnetic powder is mainly made of Fe which is surface-treated with a silane coupling agent, and contains Co of 20-50 at.% in terms of atomic percentage of Co/Fe, Al of 5-30 at.% in terms of atomic percentage of Al/Fe, and one or two or more kinds of rare earth elements R (including Y) of 4-20 at.% in terms of atomic percentage of R/Fe. The average grain diameter is less than 80 nm, a TAP density is 0.7g/cm3 or above, an ignition point is 165°C or above, and an oxygen content is 26 wt.% or less.


您还没有登录,请登录后查看详情



举报收藏 0打赏 0评论 0
本类推荐
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报