METHOD OF MANUFACTURING RARE EARTH MAGNET
2022-06-06
3950
493K
0
A manufacturing method includes : manufacturing a sintered compact having a composition of (Rl)x(Rh)yTzBsMt; manufacturing a precursor by performing hot deformation processing on the sintered compact; and manufacturing a rare earth magnet by performing an aging treatment on the precursor in a temperature range of 450° C. to 700° C. In this method, a main phase thereof is formed of a (RlRh)2T14B phase. A content of a (RlRh)1.1T4B4 phase in a grain boundary phase thereof is more than 0 mass % and 50 mass % or less. Rl represents a light rare earth element. Rh represents a heavy rare earth element. T represents a transition metal. M represents at least one of Ga, Al, Cu, and Co. x, y, z, s, and t are percentages by mass of Rl, Rh, T, B, and M. x, y, z, s, and t are expressed by the following expressions : 27≤x≤44, 0≤y≤10, z=100−x−y−s−t, 0.75≤s≤3.4, 0≤t≤3.