Soft magnetic alloys and magnetic components
2022-06-02
3380
4382K
0
[Problem] We provide a soft magnetic alloy with high saturation magnetic flux density Bs and high corrosion resistance at the same time. Solution : (Fe (1-(α + β)) CoαNiβ) 1-γX1γ) (1-(a+b+c+d+e)) BaPbSicCdCre (atomic number ratio) Is a soft magnetic alloy comprising Mn. X1 is one or more selected from Ti, Zr, Hf, Nb, Ta, Mo, W, Al, Ga, Ag, Zn, S, Ca, Mg, V, Sn, As, Sb, Bi, N, O, Au, Cu, rare earth element, and platinum group element. a to e, α to γ are within a predetermined range. The content of Mn is as f (at%), and 0. 002≦f<3. It is 0. The corrosion potential is -630mV or more -50mV or less, and the corrosion current density is 0.00 mV. It is 3 μA / cm 2 or more and 45 μA / cm 2 or less. [Selection Figure]Figure 5