METHOD FOR MANUFACTURING RARE EARTH SINTERED MAGNET

2022-05-31 3260 1037K 0
[Solution] R 1 2 T14X composition (R 1 is at least one type of rare earth element and Pr and / or nd is mandatory, T is at least one type of Fe, Co, Al, Ga, Cu and Fe is mandatory, X is boron and / or carbon) The process of obtaining R1 -T-X based sintering in which the main gravity, alloys containing R2, M and B (R 2is at least one type of rare earth element and Dy and / or Tb are mandatory, M comprises the process of obtaining a powder of at least 1 type of Fe, Cu, Al, Co, Mn, Ni, Sn, Si, B is boron), the process of presenting the alloy powder on the surface of the sintering body, the process of heating the alloy powder and the sintering agent, and the alloy comprises R2 of 5 to 60at%, 5 to 70at% M, 20at% and less than 70at% B. [Effect] It is possible to increase the coercivity while inhibiting the decrease in the residual flux density by the granular diffusion treatment, and the rare earth sintering magnet compatible with the high residual flux density and the high coercivity can be manufactured productively.


您还没有登录,请登录后查看详情



举报收藏 0打赏 0评论 0
本类推荐
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报